This rots.  I've used pull pull forever and switched to the deps system due to heavy promotion by Mike Harrison and Bryan Hebert.  They say it will be more precise.  Can anyone corroborate this?  I'd hate to switch to a system that has more downside than upside.
--Lance
  ----- Original Message ----- 
  From: Gray E Fowler 
  To: NSRCA Mailing List 
  Sent: Monday, May 08, 2006 10:51 AM
  Subject: Re: [NSRCA-discussion] Elevator trim change



  Fiberglass laminate CTE = 6 X10 -6/in/in/F 

  CF pushrod CTE = 1 X 10 -6 /in/in/F  ....could actually be 0 if fiber vloume is > 58% an all uni fibers 






  Gray Fowler
  Principal Chemical Engineer
  Composites Engineering


------------------------------------------------------------------------------


  _______________________________________________
  NSRCA-discussion mailing list
  NSRCA-discussion at lists.nsrca.org
  http://lists.nsrca.org/mailman/listinfo/nsrca-discussion
-------------- next part --------------
An HTML attachment was scrubbed...
URL: http://lists.nsrca.org/pipermail/nsrca-discussion/attachments/20060509/42b4e906/attachment.html 


More information about the NSRCA-discussion mailing list