<div>Sorry Im late into this thread but I gather the bottle cap is being used. And further I guess the threads arent shrinking so the seal is maintained?</div>  <div>&nbsp;</div>  <div>I might try and cook one up in a 215 oven immersed and filled w/ water.<BR><BR><B><I>Rcmaster199@aol.com</I></B> wrote:</div>  <BLOCKQUOTE class=replbq style="PADDING-LEFT: 5px; MARGIN-LEFT: 5px; BORDER-LEFT: #1010ff 2px solid">  <META content="MSHTML 6.00.2900.2802" name=GENERATOR><FONT id=role_document face=Arial color=#000000 size=2>  <DIV>  <DIV>Stress relief is a time-temp-chemistry sort of thing. Given the chance, PET will try to return to near it's original shape which was a thin walled, sealed at the far end, cylinder of plastic. If you weren't careful with the oven, you could potentially bring the thing all the way back. </DIV>  <DIV>&nbsp;</DIV>  <DIV>What Jim is doing is a more controlled shrink down. Working with&nbsp; the oven will work but takes more care.</DIV>  <DIV>&nbsp;</DIV> 
 <DIV>&nbsp;It may make&nbsp;some sense to fill the bottle halfway with&nbsp;water,&nbsp;make sure the cap has a hole drilled in it and then stick it&nbsp;in a pot of boiling water and cover but making sure the bottle doesn't tip over. You want the internal&nbsp; pressure build up to be eliminated but you also want thread protection. Boil it for some time and then see how it shrinks. It will stress relieve and become stable quicker probably. Haven't done that myself but could be worth a try. GL</DIV>  <DIV>&nbsp;</DIV>  <DIV>Matt</DIV>  <DIV>&nbsp;</DIV>  <DIV>&nbsp;</DIV>  <DIV>&nbsp;</DIV>  <DIV>&nbsp;</DIV>  <DIV>In a message dated 2/16/2006 9:54:37 PM Eastern Standard Time, brian_w_young@yahoo.com writes:</DIV>  <BLOCKQUOTE style="PADDING-LEFT: 5px; MARGIN-LEFT: 5px; BORDER-LEFT: blue 2px solid"><FONT style="BACKGROUND-COLOR: transparent" face=Arial color=#000000 size=2>  <DIV>Could you warm that material in an oven to acheive the same result?</DIV>  <DIV>&nbsp;</DIV>  <DIV>Maybe
 fill it w/ something to hold the shape but let it shrink.<BR><BR><B><I>Rcmaster199@aol.com</I></B> wrote:</DIV>  <BLOCKQUOTE class=replbq style="PADDING-LEFT: 5px; MARGIN-LEFT: 5px; BORDER-LEFT: #1010ff 2px solid">  <META content="MSHTML 6.00.2900.2802" name=GENERATOR><FONT face=Arial color=#000000 size=2>  <DIV>  <DIV>Jimmy, pretty much all of those pop blow molded bottles are made of PET. A fine, very tough and resilient&nbsp;engineered plastic with terrific memory built in (beats heck out of my memory, fer shure). What you experienced is completely expected.</DIV>  <DIV>&nbsp;</DIV>  <DIV>Matt</DIV>  <DIV>&nbsp;</DIV>  <DIV>&nbsp;</DIV>  <DIV>In a message dated 2/16/2006 5:16:58 PM Eastern Standard Time, jivey61@bellsouth.net writes:</DIV>  <BLOCKQUOTE style="PADDING-LEFT: 5px; MARGIN-LEFT: 5px; BORDER-LEFT: blue 2px solid"><FONT style="BACKGROUND: none transparent scroll repeat 0% 0%" face=Arial color=#000000 size=2>  <DIV>Wayne</DIV>  <DIV>&nbsp;I just flew the coke bottle tank
 today and I get 15 minutes on 24 oz of fuel.It actually draws fuel down to 1 oz in the tank,doing the Masters pattern.</DIV>  <DIV>The upside is I don't have to fill it full to complete the pattern. The weight savings is 2.5 oz using this tank.</DIV>  <DIV>&nbsp;To review...... this was a 33 oz, 1 liter coke bottle' that I pickled with 30 % heli for 2 months.</DIV>  <DIV>&nbsp;</DIV>  <DIV>Jim Ivey</DIV></FONT></BLOCKQUOTE></DIV></FONT></BLOCKQUOTE></FONT></BLOCKQUOTE></DIV>  <DIV></DIV>  <DIV>&nbsp;</DIV></FONT>_______________________________________________<BR>NSRCA-discussion mailing list<BR>NSRCA-discussion@lists.nsrca.org<BR>http://lists.nsrca.org/mailman/listinfo/nsrca-discussion</BLOCKQUOTE><BR><p>
                <hr size=1>Relax. Yahoo! Mail 
<a href="http://us.rd.yahoo.com/mail_us/taglines/virusall/*http://communications.yahoo.com/features.php?page=221">virus scanning</a> helps detect nasty viruses!