I was told that if the ratio is one-to-one, fillers have been added.
Kurt
_____
From: nsrca-discussion-bounces at lists.nsrca.org
[mailto:nsrca-discussion-bounces at lists.nsrca.org] On Behalf Of Stuart Chale
Sent: Saturday, July 14, 2007 6:16 PM
To: 'NSRCA Mailing List'
Subject: Re: [NSRCA-discussion] Building Question
In general I believe that the slower setting epoxies are stronger.
Stuart
_____
From: nsrca-discussion-bounces at lists.nsrca.org
[mailto:nsrca-discussion-bounces at lists.nsrca.org] On Behalf Of Jay Marshall
Sent: Saturday, July 14, 2007 5:48 PM
To: NSRCA
Subject: [NSRCA-discussion] Building Question
Is there any difference, other than working time, among epoxies with
different setup times but the same brand? Is 5 min just as strong as 30 min?
Jay Marshall
-------------- next part --------------
An HTML attachment was scrubbed...
URL: http://lists.nsrca.org/pipermail/nsrca-discussion/attachments/20070715/0d1a0c22/attachment.html
More information about the NSRCA-discussion
mailing list