[NSRCA-discussion] Monokote on Monokote
george w. kennie
geobet at gis.net
Mon Feb 19 12:24:10 AKST 2007
Re: [NSRCA-discussion] Monokote on MonokoteYeah Dave,
Me too. Another thing that you can't do with the new formulation is make it stick to Concept paint. Bummer !
G.
----- Original Message -----
From: k6xyz
To: 'NSRCA Mailing List'
Sent: Sunday, February 18, 2007 5:44 PM
Subject: Re: [NSRCA-discussion] Monokote on Monokote
Just curious George...I'm probably gonna use UK next time.
I started having trouble with MK in 2000 or 2001..now it won't work at all for me.
Too bad..it was great stuff.
Regards
Dave Harmon
NSRCA 586
K6XYZ[at]sbcglobal[dot]net
Sperry, Ok.
-----Original Message-----
From: nsrca-discussion-bounces at lists.nsrca.org [mailto:nsrca-discussion-bounces at lists.nsrca.org] On Behalf Of george w. kennie
Sent: Sunday, February 18, 2007 4:36 PM
To: NSRCA Mailing List
Subject: Re: [NSRCA-discussion] Monokote on Monokote
Yup, used it b/4 the new formulation and it makes for a very strong bond, but you only get one chance to get the position right. Once it's down, it ain't coming up.
G.
----- Original Message -----
From: k6xyz
To: 'NSRCA Mailing List'
Sent: Sunday, February 18, 2007 4:12 PM
Subject: Re: [NSRCA-discussion] Monokote on Monokote
I have a bottle of some kind of liquid to attach MK over MK but I've never tried it.
Has anyone used it and how did you like it?
Regards
Dave Harmon
NSRCA 586
K6XYZ[at]sbcglobal[dot]net
Sperry, Ok.
-----Original Message-----
From: nsrca-discussion-bounces at lists.nsrca.org [mailto:nsrca-discussion-bounces at lists.nsrca.org] On Behalf Of Mark Atwood
Sent: Sunday, February 18, 2007 2:04 PM
To: NSRCA Mailing List
Subject: Re: [NSRCA-discussion] Monokote on Monokote
Can it be too cold to build???
Windex is definitely the best of those three. I've had very good results with even semi large pieces (maybe 4" wide...anything wider and I'll typically only do one layer). Don't skimp on the windex. Both layers of monokote have to be clean...any dust will show up as a bump under the film. I coat both the piece I'm putting down, as well as the surface I'm putting it on, with a brush. Spraying it doesn't get enough on (unless you go crazy) and just creates a million air bubbles rather than a smooth film of liquid. I have it sloppy wet...then slide the pieces into position, and I use a small 4" shower squeegee to squeeze the windex out. You'll have zero bubbles...and it will adhere from suction pretty aggressively. Yes...you'll have a wet mess so a few paper towels are in order. Wait at least 24 hours and then use an iron set just warm enough to anchor Monokote to Monokote without any shrinking.
If you heat it too soon (same day) there's enough moisture still trapped between the two layers that you'll vaporize it and cause a bazillion bubbles.
-Mark
On 2/18/07 12:55 PM, "Ed White" <edvwhite at sbcglobal.net> wrote:
OK, Question for those finding it too cold to build. Is it possible to put monokote on top of monokote and get decent results? Tried the poke holes and windex/soap methods and not impressed with the results. Any other ideas?
Ed
ORLANDO FRETS <ojfrets at earthlink.net> wrote:
Temperature in low 30's. It's cold! It's also too cold to build, shop is cold. Stay inside where it's warm.
ORLANDO FRETS
ojfrets at earthlink.net
----------------------------------------------------------------------------
_______________________________________________
NSRCA-discussion mailing list
NSRCA-discussion at lists.nsrca.org
http://lists.nsrca.org/mailman/listinfo/nsrca-discussion
----------------------------------------------------------------------------
_______________________________________________
NSRCA-discussion mailing list
NSRCA-discussion at lists.nsrca.org
http://lists.nsrca.org/mailman/listinfo/nsrca-discussion
------------------------------------------------------------------------------
_______________________________________________
NSRCA-discussion mailing list
NSRCA-discussion at lists.nsrca.org
http://lists.nsrca.org/mailman/listinfo/nsrca-discussion
-------------- next part --------------
An HTML attachment was scrubbed...
URL: http://lists.nsrca.org/pipermail/nsrca-discussion/attachments/20070219/12075c49/attachment.html
More information about the NSRCA-discussion
mailing list